Equipment List for Iron Removal from Low-Iron Silica Sand with a Production Capacity of 20 Metric Tons Per Hour
Equipment List for Iron Removal from Low-Iron Silica Sand at a Production Rate of 20 Metric Tons Per Hour
There is only one key objective for low-iron silica sand: to reduce the iron content—and to do so consistently.A production capacity of 20 metric tons per hour (calculated based on 300 operating days per year at 20 hours per day, resulting in an annual output of approximately 120,000 metric tons) falls within the scope of a small-to-medium-sized specialized production line. While the investment threshold is moderate, the iron removal process demands a high degree of precision—if iron levels do not meet the target, achieving the desired whiteness and light transmittance is out of the question.This article outlines the configuration list for a 20-metric-ton-per-hour low-iron silica sand production line, organized by iron removal process modules.
I. First, Clarify the Iron Removal Targets and the Form in Which Iron Exists
The prerequisite for the configuration list is to clarify two things: the target iron content and the form in which iron exists.
In terms of target specifications, photovoltaic glass sand and ultra-white glass sand typically require Fe₂O₃ ≤ 0.008% (80 ppm), while optical glass sand has even stricter requirements (≤ 0.0015%). Production lines with a capacity of 20 metric tons per hour are generally positioned at the photovoltaic/ultra-white glass sand grade.
The form in which iron is present determines the required process intensity: Surface iron films and clay-like impurities can be removed using scrubbing agents; weakly magnetic associated minerals (tourmaline, hornblende) require high-gradient magnetic separation combined with flotation; while lattice impurities and fine inclusions must undergo a coupled calcination-acid leaching process.The configuration of the equipment list must be based on mineral processing tests that clarify the state of iron occurrence; otherwise, rework may be required due to situations where “magnetic separation removes the iron but the iron content still cannot be reduced.”
II. Iron Removal Configuration List (in Process Order)
1. Scrubbing and Desliming Section (Pre-treatment Iron Removal)
- High-intensity scrubbing machines: 1–2 units, sized for a processing capacity of 20 metric tons per hour, equipped with proprietary scrubbing reagents to strip surface iron film and clay
- High-efficiency agitation tank: For dispersing the chemical agent
- Hydraulic cyclone bank and desliming hopper: to remove iron-containing fine slime
- Bucket-wheel Sand Washer: Auxiliary water washing
2. Screening and Grading Section
- Circular Vibrating Screens, High-Frequency Vibrating Screens: Screen meshes configured according to target particle size; perform grading while simultaneously assisting in impurity removal
- Square Swinging Screen (for precise gradation; configured based on product requirements)
3. Magnetic Separation and Iron Removal Section (Core)
- Flat-bed Magnetic Separator (6,000 Gs class): Rough separation, 1–2 units
- Vertical-ring high-gradient magnetic separators: scavenging/refining, 1–2 units, for weakly magnetic iron-bearing minerals
- Electromagnetic Slurry Separator: For deep iron removal; 1 unit configured based on specification requirements
- Configuration Principles: Multi-stage, tiered arrangement; a combination of roughing, scavenging, and concentrating; parallel equipment ensures continuous operation during maintenance of individual units
4. Flotation Purification Section (in conjunction with iron removal)
- Aerated mechanical agitation flotation cells: 1 set, using ElevateSilica\'s proprietary flotation reagents to separate quartz from feldspar, mica, and iron-bearing minerals
- Automated Reagent Dosing System: Ensures stable reagent dosing
- Slurry adjustment tanks, concentrate/tailings thickeners: provided as supporting equipment
5. Acid Leaching Section (configured based on specifications)
- If iron levels still do not meet standards after magnetic separation and flotation, acid leaching reactors (with corrosion-resistant linings), counter-current scrubbing towers, and belt filters will be installed
- Waste acid neutralization tank, negative-pressure absorption tower for fluoride-containing exhaust gas: Mandatory environmental protection components
- Note: In regions with strict environmental regulations, prioritize the “magnetic separation + proprietary flotation” process over the acid leaching scheme
6. Dewatering and Drying Section
- Thickener, filter press, dewatering screen, dryer: Select models based on processing capacity
7. Auxiliary and Control Systems
- Pumps, Piping, Valves: Flow-through components made of high-chromium alloy or wear-resistant rubber
- Electrical Control and Automation Systems: Stable control of magnetic field strength and chemical dosing
- Dust collection system, water recirculation system
III. Key Configuration Points and Tips for Avoiding Pitfalls
Configure based on ore characteristics, not inventory. Whether to use a 2-stage or 3-stage magnetic separation process, whether flotation is necessary, and whether acid washing is required should be determined by test data to avoid over-capacity or under-capacity.
Allow for capacity margin. Select equipment for each stage at 1.1–1.2 times the 20 metric tons per hour capacity; install multiple units of critical equipment (such as magnetic separators) in parallel to ensure continuous operation.
Calculate raw ore processing capacity based on the finished product output. If the finished product output is 20 metric tons per hour, the raw ore processing capacity should be configured at 22–28 metric tons per hour.
Plan environmental protection measures concurrently. Design and invest in the treatment of waste acid and exhaust gases generated by the acid leaching process simultaneously with the main project.
IV. Recommendations for the Next Steps
A precise equipment list must be derived from beneficiation tests conducted on representative ore samples (typically 30–45 days). The test report will directly provide the recommended process flow, equipment selection list, and preliminary budget. Initial testing and design fees can be fully offset against the cost of subsequent equipment or EPC contracts.It is recommended to send samples as early as possible to initiate testing, after which the list and quotation will be issued based on actual results.
The core of the iron removal configuration for low-iron silica sand (20 metric tons per hour) is to first determine the form of iron (surface iron film, weakly magnetic associated minerals, or lattice inclusions) through mineral processing tests, and then configure equipment in modules according to the sequence “scrubbing and desliming → screening → magnetic separation → flotation → acid washing(depending on specifications) → dewatering and drying.” The magnetic separation process should feature multi-stage cascading, with key equipment configured in parallel to allow for operational flexibility, and environmental protection facilities planned concurrently.